Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG10 BK23346 - PA6-GF50 - BASF

Material Data Center offers the following functions for Ultramid® B3WG10 BK23346:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Glass fibre reinforced and heat ageing resistant injection moulding grade with excellent flowability for structural parts requiring very high rigidity. The product has a LS coloration (Laser Sensitive) and can be marked with Nd:YAG lasers.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 25 / * cm³/10min ISO 1133
온도 275 / * °C -
하중 5 / * kg -
성형 수축률, 평행 0.3 / * % ISO 294-4, 2577
성형 수축률, 수직 0.7 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 16800 / 10900 MPa ISO 527
파단시 강도 245 / 160 MPa ISO 527
파단시 신율 2.7 / 5.1 % ISO 527
챠피 충격 강도 , +23°C 105 / 105 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 90 / 90 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 18 / 25 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 15 / 15 kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 220 / * °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 210 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 220 / * °C ISO 75-1/-2
선형 열팽창 계수, 평행 15 / * E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 73 / * E-6/K ISO 11359-1/-2
전기적 특성건조/응축단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 4.2 / 5 - IEC 62631-2-1
소산 인자, 1MHz 190 / 880 E-4 IEC 62631-2-1
부피 저항 - / 1E10 Ohm*m IEC 62631-3-1
표면 저항 * / 1E12 Ohm IEC 62631-3-2
CTI - / 525 - IEC 60112
기타 특성건조/응축단위시험규격
물에서의 흡수성 4.8 / * % ISO 62와 유사
조건에서의 흡습성 1.5 / * % ISO 62와 유사
밀도 1580 / - kg/m³ ISO 1183
물질의 비성질건조/응축단위시험규격
ISO 데이터
점도수 120 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Processing humidity ≤0.12 % -
용융수지온도 270 - 300 °C -
성형온도 80 - 100 °C -
도표
점도-변형률 , Ultramid® B3WG10 BK23346, PA6-GF50, BASF
전단-변형률 , Ultramid® B3WG10 BK23346, PA6-GF50, BASF
응력-신율 , Ultramid® B3WG10 BK23346 (건조), PA6-GF50, BASF
시컨트탄성율-신율 , Ultramid® B3WG10 BK23346 (건조), PA6-GF50, BASF
인장탄성율-온도 , Ultramid® B3WG10 BK23346 (건조), PA6-GF50, BASF
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 검정
부가물
이형제
특별 특성
열안정성
특성
Laser Markable
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Mold temperature, range: 80 - 100 °C

PREPROCESSING
Max. Water content: 0.12%
Product is supplied in sealed containers and drying prior to molding is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 80 °C (176 °F) is recommended. Drying time is dependent on moisture level.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.

PROCESSING
Melt Temperature 270-300 °C (518-572 °F)
Mold Temperature 80-95 °C (176-203 °F)
Injection and Packing Pressure 35-125 bar (500-1500 psi)

This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics are critical, a mold surface temperature of 80-95 °C (176-203 °F) is required.

Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage.

Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.